Home --> PRODUCTS --> Copper Alloy --> Bronze alloy --> Tin bronze
Name:CuSn4Pb4Zn3
Download PDF Copy
Brief introduction: CuSn4Pb4Zn3
Bronze with tin as the main alloying element
Product Description
Service
Why choose us?
Buyers review

General

General

Property

Temperature

Value

Comment

Density

23.0 °C

7.7 - 8.7 g/cm³


Typical for Leaded Phosphor Bronze


Mechanical

Property

Temperature

Value

Comment

Elastic modulus

23.0 °C

110 - 130 GPa


Typical for Leaded Phosphor Bronze

Poisson's ratio

23.0 °C

0.33 [-]


Typical for Leaded Phosphor Bronze

Thermal

Property

Temperature

Value

Comment

Coefficient of thermal expansion

23.0 °C

1.5E-5 - 1.9E-5 1/K


Typical for Leaded Phosphor Bronze

Specific heat capacity

23.0 °C

380 J/(kg·K)


Typical for Leaded Phosphor Bronze

Chemical properties

Property

Value

Iron

0.1 %


Lead

0.05 %


Nickel

0.3 %


Other

Rest Cu

Tin

3 - 5 %


Zinc

1 - 3 %


  If you need product information or price, please fill in your contact information in the form, we will usually contact you within 12 hours. You could also email me info@lyapm.com to get prompt reply.


Special recommendation
5052 Aluminium
SUP9 Spring Steel | 55CrMnA | 55Cr3 | 1.7176 | 527A60
7075-t6 aluminum pipe
5754 aluminium alloy
6061 T6/T651 ALUMINIUM PLATE
CuZn36Pb3 (CW603N) lead brass
CONTACT US
NO.501 Dongshe Road, Dongjing Town, Songjiang District, Shanghai,China,201600
Mobile/Whatsapp/Zalo/Lines/Skype:+8616628500844
Copyright@2018-2030 LUOYUE PRECISION METAL (SHANGHAI) CO., LTD