International Comparison of Materials
EU
ENINTER ISO USA
AISIJAPAN
JISGERMANY
DINCHINA
GBFRANCE
AFNORITALY
UNI-- -- D2 SKD11 X165CrMoV12 Cr12MoV -- --
SPAIN
UNESweden
SSFinland
SFSPoland
PNCzechia
CSNAustria
ONORMRussia
GOSTEngland
BS-- -- XW-41 -- -- -- BD2 --
**This comparison table is for reference only. The standards and grades of various countries have slightly different chemical compositions. Please refer to the database for details.**
Chemical Composition(JIS G4051)
C(%) Si(%) Mn(%) P(%) S(%) Ni(%) Cr(%) V(%) Cu(%) 1.4-1.6 0≦0.4 0≦0.6 0≦0.03 0≦0.03 0≦0.5 11.0-13.0 0.2-0.5 0≦0.25 Conditions of heat treatment
Criterion for heat treating conditions revise:
Mechanical properties
Tensile strength (kgf/mm²): 128
Yield strength (kgf/mm²): 103
Elongation (%): 15.6
Cross section reduction rate (%): 38
Impact value (J/cm2): 2
Hardness (Hb) : 41
Size Range
Shape Size(mm) Round Bar 8.2, 9.2, 10.2, 11.2, 12.2, 13.2, 14.2, 15.2, 16.2, 17.2, 18.2, 19.2, 20.2, 22.2, 24.2, 25.2, 26.2, 28.2, 30.2, 32.2, 34.2, 36.2, 38.2, 40.2, 42.2, 44.2, 46.2, 48.2, 51, 56, 61, 66, 71, 76, 81, 86, 91, 96, 101, 111, 121, 131, 141, 151, 161, 171, 181, 191, 201, 211, 221, 231, 241, 251, 261. If you need product information or price, please fill in your contact information in the form, we will usually contact you within 12 hours. You could also email me info@lyapm.com to get prompt reply.