Chemical Composition of Tool Steel H11

Element Min (%) Max (%)
Carbon, C 0.38 0.43
Manganese, Mn 0.20 0.40
Silicon, Si 0.80 1.00
Sulfur, S 0.015
Phosphorus, P 0.015
Chromium, Cr 4.75 5.25
Molybdenum, Mo 1.20 1.40
Vanadium, V 0.40 0.60
Nickel, Ni 0.25
Copper, Cu 0.35
Iron, Fe *Balance

*Not exclusively to the element mentioned, but that one predominates other elements that are used only in minimal quantities.

Fabrication and Working Instructions

Tool Steel H11 can be easily formed using conventional methods for machining and forging. For forging the preferred temperature is 2050° F (1121° C), with 1650° F (899° C) being the lowest recommended point. H11 can also be cold-worked and welded with conventional methods for steels in this group. That said, machinability of H11 is 75% to that of steels in the “W” group.

Mechanical and Physical Properties of Tool Steel H11

Property Imperial Metric
Density 0.282 lb/in³ 7.81 g/cc
Melting Point 2600°F 1427°C
Tensile Strength 260 ksi 1792 MPa
Tensile Strength, Yield 215 ksi 1482 MPa
Elongation in 4D 8 % 8 %
Reduction of Area 30 % 30 %
Hardness, Rockwell C
Air cooled from 1800°F (982°C) for 45 minutes)
52.5 52.5
Hardness, Rockwell C
Air cooled from 1850°F (1010°C) for 45 minutes)
56 56
Hardness, Rockwell C
Air cooled from 1900°F (1038°C) for 45 minutes)
57 57
Charpy impact
V-notch; air-cooled from 1850°F (1010°C) and then tempered at 535°C
10.0 ft-lb 13.6 J
Charpy impact
V-notch; air-cooled from 1850°F (1010°C) and then tempered at 1200°F (650°C)
20.0 ft-lb 27.1 J
Charpy impact
V-notch; air-cooled from 1850°F (1010°C) and then tempered at 700°F (370°C)
25.0 ft-lb 33.9 J
Poisson’s Ration 0.27 – 0.30 0.27 – 0.30
Machinability (relative rating for 1% Carbon Steel) 75-80 % 75-80 %

Transverse Tensile Properties

Property Imperial Metric
Tensile Strength 260 ksi 1792 MPa
Tensile Strength, Yield (0.2% Offset) 215 ksi 1482 MPa
Individual Value 6 % 6 %
Average Value 15 % 15 %

Thermal Properties of Tool Steel H11

Property Imperial Metric
Thermal Expansion
(at the temperature range of 68-112° F / 20-100° C)
6.63 µin/in°F 11.9 x 10-6/ºC
Thermal Conductivity(at 212° F / 100° C) 292.9 in/hr.ft².°F 42.2 W/mK

 If you need product information or price, please fill in your contact information in the form, we will usually contact you within 12 hours. You could also email me info@lyapm.com to get prompt reply.

Special recommendation
5052 Aluminium
SUP9 Spring Steel | 55CrMnA | 55Cr3 | 1.7176 | 527A60
7075-t6 aluminum pipe
5754 aluminium alloy
6061 T6/T651 ALUMINIUM PLATE
CuZn36Pb3 (CW603N) lead brass
CONTACT US
NO.501 Dongshe Road, Dongjing Town, Songjiang District, Shanghai,China,201600
Mobile/Whatsapp/Zalo/Lines/Skype:+8616628500844
Copyright@2018-2030 LUOYUE PRECISION METAL (SHANGHAI) CO., LTD