Home --> PRODUCTS --> Stainless Steel --> Martensite stainless steel
Name:SUS420JI
Download PDF Copy
Brief introduction: SUS420JI
astm aisi 420 jis sus420ji 430j2 stainless steel sheet
Product Description
Service
Why choose us?
Buyers review

  

What is SUS420JI stainless steel? 


SUS420(2Cr13) steel has high toughness, high hardness, air-cooled hardened high chromium tool steel, better hardness and toughness than SKD steel, high mirror surface, high corrosion resistance. The size change of heat treatment is small.


SUS420JI  steel should belong to stainless steel from the classification, more accurate classification should be attributed to martensitic stainless iron, mainly used for mechanical processing, better than normal stainless steel cost performance, so in the case of low corrosion resistance requirements, has been more widely used. SUS420JI has better mechanical properties and machinability after quenching treatment, and its microstructure is Martensite shape.




The corresponding brand of SUS420JI is as follows:

1. Corresponding standard brand: GB/T1220-2007;
2, corresponding to the Japanese brand: SUS420JI;
3, corresponding to the German brand: X20CR13/1.4021;
4, corresponding to the American brand: 420

2Cr13 (new number: 20Cr13) Standard: GB/T 1220-2007


     



Characteristics and application: high hardness and good corrosion resistance under quenching state. Used as turbine blades. 2Cr13 density 7.75g/cm3 2Cr13 quenching hardness: generally, the quenching temperature of 2Cr13 is 980 ~ 1050℃, the hardness of oil quenching at 980℃ is significantly lower than that at 1050℃, the hardness of oil quenching at 980℃ is 45 ~ 50HRC, and the hardness of oil quenching at 1050℃ is 2HRC higher. However, the microstructure obtained after quenching at 1050℃ is coarser and more brittle. It is recommended to use 1000℃ heating quenching can get better microstructure and hardness. 2Cr13 Martensitic stainless steel, preheated for welding. And Q235 austenitic stainless steel welding rod without preheating, such as A302.A307 can be. Weld dilution rate is controlled during welding, welding without swing, and small current is used.
2Cr13 welding material can be selected:
1. Atmospheric corrosion resistance G202,G207, need to preheat 150-300 degrees, after welding 700-730 degrees tempering;
2. Resistance to organic acid and heat resistance: G211, need to preheat 150-300 degrees;
3. Good plasticity: A102 A107, A202, A207, A302, A307, repair welding preheating, thick big preheating



2Cr13 chemical composition 
Carbon C: 0.16 ~ 0.25
Si Si: 1.00 or less
Manganese Mn: 1.00 or less
S: sulfur 0.030 or less
P P: 0.035 or less
Chromium Cr: 12.00 ~ 14.00
Nickel Ni: allowable content ≤0.60



Mechanical properties of
Tensile strength σ B (MPa) : quenched temper,≥640
Condition yield strength σ0.2 (MPa) : quenched and tempered,≥440
Elongation δ5 (%) : quenching and tempering,≥20ψ (%) 
quenched and tempered,≥50
Impact energy Akv (J) : quenching and tempering,≥63
Hardness: Annealing,≤223HB; Quenching and tempering,≥192HB

Heat treatment specification and metallographic structure
Heat treatment
1) Annealing, slow cooling at 800 ~ 900℃ or fast cooling at about 750℃;
2) quenching, oil cooling at 920 ~ 980℃;
3) Tempering,600 ~ 750℃ fast cooling.
Metallographic structure: The structure is characterized by Martensite type.

Delivery status:
Generally, the goods are delivered in the condition of heat treatment, and the type of heat treatment is indicated in the contract. If it is not indicated, the goods will be delivered without heat treatment.

Main uses:
1, mechanical structure parts, engine exhaust pipe, boiler combustion chamber, burner.
2, building exterior decoration materials, car parts, cold and hot water supply equipment.
3, used in grain boundary corrosion resistance of chemical, coal, oil industry outdoor open-air machine, building materials heat-resistant parts and parts with difficulty in heat treatment.
Welding materials:
1, atmospheric corrosion resistance G202, G207, need to preheat 150-300 degrees, after welding 700-730 degrees tempering;
2, organic acid resistance and heat resistance G211, need to preheat 150-300 degrees;
3, good plasticity: A102, A302, A307, repair welding preheating, thick parts preheating.


If you need product information or price, please fill in your contact information in the form below, we will usually contact you within 12 hours. You could also email me info@lyapm.com to get prompt reply.

Special recommendation
5052 Aluminium
SUP9 Spring Steel | 55CrMnA | 55Cr3 | 1.7176 | 527A60
7075-t6 aluminum pipe
5754 aluminium alloy
6061 T6/T651 ALUMINIUM PLATE
CuZn36Pb3 (CW603N) lead brass
CONTACT US
NO.501 Dongshe Road, Dongjing Town, Songjiang District, Shanghai,China,201600
Mobile/Whatsapp/Zalo/Lines/Skype:+8616628500844
Copyright@2018-2030 LUOYUE PRECISION METAL (SHANGHAI) CO., LTD